Joint Filling Plaster is used for in filling of joints between adjacent plasterboard.
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust.
User Instructions:
Put some water in a clean container. Wait two minutes and mix Joint Filling Plaster with water with some sort of mixing tool until they homogenize. It is very important that water, mixture container and tools are clear.
With increased heat and sound insulation properties It is applicable for concrete, gross concrete, gas-concrete, bims and
brick surfaces.
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust. The surfaces (brick,concrete,and gas concrete) must be wet before application.
User Instructions:
Put some water in a clean container. Sprinkle plaster on water until the plaster float on water. Wait 2-3 minutes for getting wet plaster and mix plaster with water with some sort of mixing tool until they homogenize. It is very important that water, mixture container and tools are clear.
Regarding to its thickness and homogenous of freezing time more, it is used for decorating ceiling and carton pierre.
Properties of Application Surface:
Moulds must be perfectly dry before mounting.
User Instructions:
Put some water in a clean container. Sprinkle plaster on water until the plaster float on water. Wait 2-3 minutes for getting wet plaster and mix plaster with water with low-period mechanic mixing tool until they homogenize. After mixturing, mixture is ready for falling on moulds. Mixture freezes within 20 minutes. It is very important that water, mixture container and tools are clear.
With increased heat and sound insulation properties It is applicable for concrete, gross concrete, gas-concrete, bims and
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust. Smooth surface must be formed on application surface. The surfaces (brick,concrete,and gas concrete) must be wet before application.
User Instructions:
Appropriate water-plaster ratio is regulated with plaster machine. In all application plaster thickness must be 1.5 cm. Regarding to this thickness anos are settled with interval which must not be greater then used gauge height. The mixture which made by plaster machine is sprayed between anos. The filled surface is made smooth and extra mixture is taken from the surface. After this process the mixture which is on surface is left and passed the other empty anos. Before starting to make plaster mixture pre-setting, the surface is polished with trowel. Approximately after one hour water is sprinkled on the polished surface. The surface is shined with trfil and polished with trowel again.
It is applied on gros concrete surfaces, plaster and dark plaster. It makes surface smoothed and forms suitable surface for plastic paint, oil paint or wallpaper.
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust.
User Instructions:
Put 6-7 liter water in a clean container. Sprinkle plaster on water until the plaster float on water. Wait 2-3 minutes for getting wet plaster and mix plaster with water with some sort of mixing tool until they homogenize. It is very important that water, mixture container and tools are clear.
It is used in filling of joints of gypsum wallboards and thermal insulations.
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust.
User Instructions:
Put 6-7 liter water in a clean container. Sprinkle plaster on water until the plaster float on water. Wait 2-3 minutes for getting wet plaster and mix plaster with water with some sort of mixing tool until they homogenize. It is very important that water, mixture container and tools are clear.
Good wear resistance, easy to prepare, avoid cracks for all interior areas of floor and wall grounting of ceramic tiles, mosaics and marble for 1-6 mm joints.
Properties of Application Surface:
The joints must be clean and free of dust. It is advised to dampened with a wet sponge. Wait until adhesive has completely achieved sufficient hardness.
User Instructions:
Pour mostar into 6-7 liters of clean water slowly and mix homogeneous mixture free from lumps. It should be precisely measured that amount of water. After resting it for 5 minutes, remix it for 1-2 minutes again. Mortar is ready to use. Fill the joints completely with mortar using suitable rubber trowel and remove excess mortar from surface with diagonal moves. Wait for the settling of the material and repeat this procedure. Then, clean surface with a damp sponge give the final shape to the material. Any residue left can be cleaned from the surface with a clean dry cloth.
It can be used as a plaster for all kind of thermal insulation boards such as EPS, XPS and Rockwool.
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust. Sheets have to be strongly adhered on the surface.
User Instructions:
Pour mortar into 5,5 - 6,5 liters of clean water slowly and mix with a low speed mixer until getting homogeneous mixture free from lumps. After resting it for 5 minutes remix it for 1-2 minutes. It will be ready to use. After that, fix the mesh onto the first layer gently with steel trowel before it dries. Make overlaps for approximately 10 cm at the joints of the plaster mesh. After 3-4 hour apply the second layer of mortar.
It can be used as a plaster for all kind of thermal insulation boards such as EPS, XPS and Rockwool with its excellent bonding strength.
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust. Sheets have to be strongly adhered on the surface.
User Instructions:
Pour mortar into 5,5 - 6,5 liters of clean water slowly and mix with a low speed mixer until getting homogeneous mixture free from lumps. After resting it for 5 minutes remix it for 1-2 minutes. It will be ready to use. Apply it to the back side of the sheet as a strip and also a point on the center of the sheet. It also should be applied all around of insulation board and 5 mm of space should be left from the edges all around the board. It should be advised minimum 40% of the insulation board is covered by adhesive. After that, fix the sheets onto the wall by pressure. During installation, please check level of panels with a gauge.
With cement based ceramic tile adhesive with reduced slip properties it is applied on the cement based plaster, screed and concrete on the horizontal and vertical surfaces.
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust. Surface irregularities, cracks and holes should be repaired and the substrates must be primed before bonding of tiles on existing ceramic tiles.
User Instructions:
Pour it into 6-7 clean water slowly and mix with a low speed mixer to get a homogeneous mixture free from lumps. Allow the mortar to rest for 5 minutes and remix it again. Spread mortar onto the substrate then notch with the toothed side of trowel. Large tiles should be applied also on back of tiles within application.
With its cement based high performance adhesive with reduced slip and extended open time properties, it is used for indoor&outdoor granite and ceramic applications, swimming pools, water tanks, underfloor heating surfaces and tiles of cold storage places.
Properties of Application Surface:
All substrates must be strong, dry, clean and free from oil, grease, dust. Surface irregularities, cracks and holes should be repaired and substrates must be primed before bonding of tiles on existing ceramic tiles.
User Instructions:
Pour it into 6,5 - 7,5 liters of clean water slowly and mix homogeneous mixture free from lumps. Then rest it for 5 minutes and remix it for 1-2 minutes. It will be ready to use. Spread the mortar onto the substrate then nothc with the toothed side of trowel. Open time is 30 minutes and within this period install the tiles with pressure. It is advised to apply it for both of the surfaces for big sizes of ceramic tiles and granites.
It is applied for repairing and plastering the concrete surfaces and defects on the concrete surfaces before coating with its perfect adherence to the concrete surfaces and high thixotrophic properties.
Properties of Application Surface:
All substrates must be strong, clean, free from oil, grease, dust and dry. Low adherenced loose parts should be removed from surface and the surface should be dampened prior to the application.
User Instructions:
Pour mortar into 5,5 - 6,5 liters of clean water slowly and mix with a low speed mixer to get a homogeneous mixture. Then rest it for 5 minutes and remix it for 1-2 minutes. Repairing mortar is ready to use.